Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G45-1242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G45-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-46 |
filingDate |
2019-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b44537ad79a85dbd90762142733614e3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dfcc841e056e82ce8339c46b3132b291 |
publicationDate |
2021-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20210021730-A |
titleOfInvention |
Method for preparing lithium manganese oxide based positive electrode active material |
abstract |
The present invention relates to a process for producing a γ-MnOOH at normal pressure and a temperature not higher than 100 ℃, and this produced a phase change that then, the β-MnO 2 lithium manganese oxide-based positive electrode active material by using a β-MnO 2 . |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115286051-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115286051-A |
priorityDate |
2019-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |