http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200128202-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4e58a7247d4c843be828cff866761ddd |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1837 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-2073 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-20 |
filingDate | 2017-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_41a6c4e361a6ff9c3bfd2297a7a45cfc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0a36d3bcde7ed150eff2eba86eaa5d55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26ac83552f0606d1b866bb474d2d75d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92b11282056e951ae88fee6f3548a4ef |
publicationDate | 2020-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20200128202-A |
titleOfInvention | Nickel colloidal catalyst solution for electroless nickel or nickel alloy plating, and method for electroless nickel or nickel alloy plating |
abstract | After immersing a non-conductive substrate in a surfactant-containing solution to promote adsorption, a colloidal stabilizer (C) consisting of soluble nickel salt (A) and a reducing agent (B) and specific sugars such as glucose, fructose, sorbitol, xylitol, maltitol, and mannitol. ), a catalyst is applied to a non-conductive substrate with a nickel colloidal catalyst solution for electroless nickel plating containing ), and then electroless nickel plating is performed. After enhancing the catalytic activity by the adsorption promoting treatment, the catalyst is applied with a nickel colloid catalyst solution having excellent aging stability and repetition resistance, and subjected to electroless nickel plating, so that a uniform nickel film without uneven precipitation can be obtained. Even if a nickel alloy plating method is applied instead of the nickel plating method, a nickel alloy film having excellent uniformity can be obtained. |
priorityDate | 2016-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |