Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b0a261eb618936fac30c812fcb9d3ad3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3418 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3272 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3217 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B23-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-632 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-6261 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62655 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62635 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-632 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-626 |
filingDate |
2019-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7af12d48037636f4a837268a8deedc4f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8645a2ce2b61ab525542c1548a55a51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df7df1da8ceb2a3e6785fa8323d48d03 |
publicationDate |
2020-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20200090320-A |
titleOfInvention |
Manufacturing Method and Compositions for Power Saving Matter by using SiO₂, Al₂O₃, Fe₂O₃ and Vinyl Acetate |
abstract |
According to the method of manufacturing a power saver material of the present invention, silicon dioxide (SiO 2 ) in the range of 30 to 45 weight percent (wt(%)) and aluminum oxide (Al 2 ) in the range of 20 to 30 weight percent (wt(%)) O 3 ) and a mineral containing iron oxide (Fe 2 O 3 ) in the range of 20 to 35 weight percent (wt(%)) are prepared, and the prepared mineral is crushed in the range of 80 to 200 mesh to make the mineral powder. Produced, and mixed with an eco-friendly binder material containing vinyl acetate, ethanol, ethyl acetate and the produced mineral powder to a predetermined mixture content ratio range while stirring to liquefy the liquid phase. Create a mixture, inject the liquid mixture into a mold having at least two highly conductive electrode parts arranged to be insulated from each other in a specified geometric relationship in a housing space of a specified geometry, and dry the liquid mixture injected into the fabrication frame at room temperature To produce a cured power saver material. |