Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_eeabb570cbfa42bdc37ecdc5ef9f6392 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-9083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-88 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-88 |
filingDate |
2018-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bf63b1a255cd50eee411f59b1a5885e3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b158463586b7f9f0dd2b1a1cb611304 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_851b51ec951c4e3a292dc0e277b94485 |
publicationDate |
2020-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20200040354-A |
titleOfInvention |
Method of producing carbon-supported cobalt pentlandite by pyrolysis and carbon-supported cobalt pentlandite by the method |
abstract |
The present invention comprises the steps of forming a homogenate by mixing lignin and cobalt oxide; And thermally decomposing the homogenate under a carbon dioxide atmosphere at a temperature of 700 ° C. or higher to produce cobalt pentlandite supported by a carbon support; wherein the carbon-supported cobalt pentlandite is produced. to be. |