abstract |
The present invention provides a composition for the preparation of a thermoplastic molding compound, wherein the composition is selected from the group consisting of the following components: A) 30 to 90% by weight of an aromatic polycarbonate, an aromatic polyester carbonate and an aromatic polyester At least one polymer, B) from 5 to 65% by weight of an epoxy group-free polymer, wherein B.1) rubber-modified vinyl (co) polymers prepared by the emulsion polymerization process, and B.2) optionally rubber- Polymers consisting of vinyl-free (co) polymers, C) block polymers or graft polymers containing 0.5 to 10% by weight of structural elements derived from styrene and at least one epoxy-group-containing vinyl monomer, D) Contain or consist of 0.001 to 20% by weight of one or more additional additives, wherein component C is a structural element versus epoxy derived from styrene of 100: 1 to 1: 1; Having a weight ratio of structural elements derived from -group-containing vinyl monomers, wherein at least one of the composition components contains Bronsted-acidic and / or Bronsted-basic compounds. The present invention relates to a method for producing a molding compound from a composition, the molding compound itself, the use of the composition or molding compound for producing the molding, and the molding itself. |