http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190076369-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6f932d94618d9b875e401457b33e9761 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2201-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-312 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 |
filingDate | 2017-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4e66f3a237c3c46755ff5ff28bfb762 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed1b928bbb67faef82205a2cb3308c53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6621eb0bf3783068b161eb73f7152d8d |
publicationDate | 2019-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20190076369-A |
titleOfInvention | Adhesive composition, adhesive sheet, optical member and image display device produced using the same |
abstract | The pressure-sensitive adhesive composition according to the present invention comprises an acrylic polymer; And at least one dilution monomer, wherein the non-volatilization ratio according to the following non-volatility measurement method is 98% or more, and the number of bubbles according to the below-described bubbling water evaluation method is 1.0 / cm 2 or less. [Method for measuring nonvolatile rate] After the weight (A) of the glass substrate (5 cm x 7 cm) was measured, an adhesive sheet (4 cm x 5 cm, thickness: 100 m) formed of a pressure sensitive adhesive composition formed on one side of the glass substrate was bonded and initial weight (B) , Dried at 130 캜 under vacuum condition for 1 hour, left in a desiccator for 30 minutes, and then the weight (C) is measured to calculate the non-volatile rate ((CA) / (BA) x 100). [Evaluation method of bubble generation water] PET (7 cm × 7 cm) having a thickness of 100 μm was bonded to both sides of a pressure sensitive adhesive sheet (5 cm × 5 cm, thickness: 100 μm) formed of the pressure-sensitive adhesive composition, autoclaved at 50 ° C./5 atm for 20 minutes, And the number of bubbles per unit area is confirmed. The pressure-sensitive adhesive composition according to the present invention is advantageous in that it can produce a pressure-sensitive adhesive sheet having excellent elastic modulus and low bubble generation per unit area. |