http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190060105-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8caec439897276c38167265c0de749c8 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2331-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2101-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L9-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N65-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M11-77 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N65-08 |
filingDate | 2017-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c28876ec385b1872e73f84a702d59c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ea4c198013ae4b2e6ddc2d4faa7eea2 |
publicationDate | 2019-06-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20190060105-A |
titleOfInvention | Fused composite active minerals and method for producing fibers using the same |
abstract | In the method for producing fused composite active mineral according to an embodiment of the present invention, a step of preparing a mixture by uniformly mixing silica, minerals, and sodium chloride having a silicon dioxide concentration of 99% in a mixer; Placing the mixture in a furnace and heating and melting the mixture; Placing the molten mixture in a molding machine and cooling the molten mixture to produce a solid; The solid material and the water in a melting furnace, heating and dissolving the mixture, and storing the dissolved mixture in a prepared container. In addition, in the method of preparing the fused complex active mineral fiber according to the embodiment of the present invention using the fused complex active minerals, the step of preparing mineral alkali water by diluting the fused complex active mineral with the water; Immersing the prepared fiber in the mineral alkaline water for 30 to 40 minutes, and drying the immersed fiber in sunlight. |