http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180112199-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e86afcb9962e3512083c29b5de7f6d7c
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-098
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A46D1-0207
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A46D1-006
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A46B9-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D39-1623
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-76
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-088
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A46D1-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A46B9-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D39-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-098
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-088
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-76
filingDate 2017-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c301877fe0542fc458157dd3df85113
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f160ec7812b3dbd4e7a4fa16d96c8a7f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_76568f4501eb83648f7062a6bb27683d
publicationDate 2018-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-20180112199-A
titleOfInvention Polyketone fiber and mehod of manufacturing the same and toothbrush using the same and antibacterial filter using the same
abstract A polyketone fiber capable of securing excellent durability and heat resistance by producing a polyketone fiber by extrusion-radiating a polyketone resin, a method for producing the same, a toothbrush using the same, and an antibacterial filter using the same. A method for producing a polyketone fiber according to the present invention comprises the steps of: (a) melt-extruding a polyketone resin; (b) extruding and spinning the melt extruded polyketone resin using a nozzle to form a yarn; And (c) cooling and extruding the extruded yarn to form polyketone fibers. After step (c), the polyketone fibers have an impact strength of 8 to 10 KJ / m 2 .
priorityDate 2017-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID11499
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419532347
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23954
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID450515042
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419557109
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID160986

Total number of triples: 36.