http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180108445-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8412303829f82505584efd929e126dd0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2201-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2203-318 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2433-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-408 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-20 |
filingDate | 2018-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26533b48f5aaff8548d5449b20000442 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96fc24939a76410d500461d817c7de53 |
publicationDate | 2018-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20180108445-A |
titleOfInvention | Adhesive sheet |
abstract | (assignment) Provided is a pressure-sensitive adhesive sheet having a pressure-sensitive adhesive layer having blister resistance and whitening resistance even under high-durability conditions and having good substrate adhesion. (Solution) A pressure-sensitive adhesive sheet comprising a substrate and a pressure-sensitive adhesive layer formed from the pressure-sensitive adhesive composition containing the (meth) acrylic copolymer (A) and the crosslinking agent (B) on the substrate, : (i) Adhesive strength of 10.0 N / 25 mm or more in measurement after sticking the pressure-sensitive adhesive surface of the pressure-sensitive adhesive layer to a polycarbonate plate and leaving the pressure-sensitive adhesive layer for 72 hours under an 85 ° C / 85% RH environment. (ii) a pressure-sensitive adhesive surface of the pressure-sensitive adhesive layer is attached to a polycarbonate plate in an area of 20 mm x 20 mm, and when a load of 1 kg is applied in a shearing direction under an environment of 80 캜, The displacement of the pressure-sensitive adhesive layer is 1.0 mm or less. (iii) the pressure-sensitive adhesive surface of the pressure-sensitive adhesive layer is attached to a polyethylene terephthalate film and the pressure-sensitive adhesive force is 5.0 N / 25 mm or more in the measurement after being left for 72 hours under an 85 ° C / 85% RH environment. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019085479-A |
priorityDate | 2017-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 169.