abstract |
It is an object of the present invention to provide a vinyl chloride resin composition excellent in impact resistance, workability, and heat resistance, and a molded article made of the resin composition, particularly a pipe. According to the present invention, there is provided a rubber composition which comprises 3 to 15 parts by mass of a rubber-based shock absorber (B) and 0.1 to 10 parts by mass of a modified olefin wax (C) with respect to 100 parts by mass of a vinyl chloride resin (A) (III), and a molded article, particularly a pipe, made of the resin composition. This resin composition satisfies the following requirements (I) to (III). (Tg) in the differential scanning calorimetry (DSC) of the rubber-based shock absorber (B) is 0 占 폚, the chlorine content of the vinyl chloride resin (A) is 55 to 75 mass% (III) The modified olefin wax (C) contains at least one polar group selected from halogen and carboxylic acid derivatives, and the content of the polar group is in the range of 0.1 to 50 mass%. |