Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2009-245 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2301-255 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06F2203-04112 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06F2203-04103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06F3-041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F1-0547 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F1-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B13-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 |
filingDate |
2016-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0db0e60d0ed73a2d552bc4a6e2ceb077 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d109326a2b7dbff379e73aaf5f4999ed http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cbf0b640e5a81af90677a7edbcdb15ed |
publicationDate |
2018-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20180030063-A |
titleOfInvention |
Manufacturing method |
abstract |
It is an object of the present invention to provide a method for producing a metal nanowire having a small diameter and a long length. A method for producing a metal nanowire according to the present invention is a method for producing a metal nanowire, comprising: maintaining a first solution containing an ionic derivative and a polyol as a solvent at a temperature of 80 to 200 ° C; adding a metal salt and a polyol as a solvent to a second solution , The ratio of the total number of moles of the halogen atom of the ionic derivative in the first solution to the number of moles of the metal atom of the metal salt to be supplied in one minute (moles of the metal atom of the metal salt supplied in one minute / Total number of moles) is less than 10. The ionic derivative is preferably a halide of a quaternary ammonium salt, and the metal salt is preferably nitric acid. |