abstract |
(A) from 20% to 99.9% by weight, based on the total composition, of one or more polyamides independently selected from the group consisting of aliphatic polyamides, semiaromatic polyamides, aromatic polyamides, and blends thereof; (B) from 0.1% to 10% by weight, based on the total composition, of one or more polyether polyols having a melting temperature below room temperature; (C) from 0% to 70% by weight, based on the total composition, of one or more adjuvants; And (D) from 0% to 50% by weight, based on the total composition, of one or more other additives. Another aspect of the present invention is the use of a molded article made from the above-mentioned polyamide composition, the use of a polyether polyol to improve the melt flow of the polyamide composition, and the use of a polyether polyol It provides usages. |