http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170118187-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C47-0057 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-0018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C67-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-049 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-049 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C67-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2016-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec2c9d57a8ef4f7cd049be5c1b7bbea6 |
publicationDate | 2017-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20170118187-A |
titleOfInvention | A stretched white polyester film and a manufacturing method thereof, a back sheet for a solar cell, |
abstract | Wherein the content of the white particles with respect to the total mass of the film is from 2 to 10 mass% and the average area per one cross section in the film thickness direction is from 0.010 to 0.050 占 퐉 2 / White polyester film, and its application. The method for producing an oriented white polyester film comprises a longitudinal stretching step of stretching an unstretched white polyester film in the machine direction and first to Nth transverse stretching steps of stretching in the transverse direction, The stretching speed of the white polyester film in the width direction is increased in the transverse stretching process, the stretching temperature in the Nth transverse stretching process is set to 140 to 180 ° C, and the width of the white polyester film before the first stretching process The length in the width direction is increased by 8 to 25% per second with respect to the length of the direction. N is an integer of 2 or more, and n is an integer of 2 to N. |