Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2220-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-122 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0404 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-623 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate |
2016-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc2124695875c16e91c3ff76cb0d6c71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fbd56bf9de8d9b626f51e013c7c011d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_95f46598007ed6b5a38895103954a835 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_135a980597341abb3cf720997a1938a6 |
publicationDate |
2017-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20170111722-A |
titleOfInvention |
Method of preparing electrode slurry for a lithium secondary battery |
abstract |
The present invention relates to a method for manufacturing an electrode slurry for a lithium secondary battery, which can minimize the drag line by improving the physical properties of the electrode slurry by performing a primary mixing process at a high viscosity by adjusting the amount of the binder, The present invention provides a method for manufacturing an electrode for a lithium secondary battery in which the electrode defective ratio is reduced using the slurry production method and the cell stability is improved, and an electrode manufactured by the method and a secondary battery including the same. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022211338-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10804528-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220135544-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220135529-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220135541-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220135539-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022244963-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018093151-A1 |
priorityDate |
2016-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |