http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170064519-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f03d8c755ecf6e58caa28ad7aa972696 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-0207 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K5-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27N1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-0278 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-0242 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27N1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K5-00 |
filingDate | 2017-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8f3953499d19b867c9a7f5f83d32a1b |
publicationDate | 2017-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20170064519-A |
titleOfInvention | Method of manufacturing loess wood |
abstract | More particularly, the present invention relates to a method for producing loess wood, which comprises a first step of producing a mixture of loess and salt mixed into particles having a size of 0.1 to 5 nm, A second step of mixing an aluminum chloride-based inorganic curing agent comprising aluminum with water to prepare a crude soil solution, a third step of introducing wood into the impregnation furnace, and applying a vacuum to the impregnation furnace to remove moisture and impurities in the interior of the wood A fifth step of supplying a loess stock solution to the storage tank of the impregnation furnace, a sixth step of applying a pressure of the impregnation furnace to permeate the loess loose solution into the interior of the wood structure, The seventh step of recovering the residue of the surface and the excessively absorbed loamy stock solution, the wood recovered from the loam soil solution is dried at a temperature of 60 to 120 ° C for 8 hours to 7 days The eighth step and to a yellow soil timber manufacturing method which comprises the ninth step of the grinding process to the surface of the dried timber. In addition, the loess wood produced according to the present invention is advantageous in that it is easy to purchase the loess, which is a raw material, because it is inexpensive in terms of industrial cost, and that it is safe in handling, and that fusing within the wood is easy due to the viscous properties of loess . In addition, it uses environmentally friendly loess to be environmentally friendly and has excellent humidity control ability. It is used with wood and has high air permeability and heat resistance. It is beneficial to human health through far-infrared radiation and can inhibit the mold growth with strong antibacterial power. There is an effect. In addition, it has a high ignition temperature due to the mixing of wood and yellow clay mineral ceramics. It plays a role of retarding or suppressing the occurrence of fire, and it has an effect of suppressing the generation of toxic gas because no flame is formed during combustion. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102524672-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109016007-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220031182-A |
priorityDate | 2017-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 234.