abstract |
The extruded water-soluble article is made of a homogeneous material comprising a water-soluble polymer having an extrusion temperature of 50 < 0 > C to 150 < 0 > C. This relatively low extrusion temperature is compatible with the active agent which otherwise would have been destroyed in the high temperature extrusion process. The article further comprises from 0.1% to 50% by weight of the active agent. Potential activators include, but are not limited to, isothiazolone, alkyldimethylammonium chloride, triazine, 2-thiocyanomethylthiobenzothiazole, methylenebistiocyanate, acrolein, dodecylguanidine hydrogen chloride, chlorophenol, quaternary ammonium salts, But are not limited to, aldehydes, dithiocarbamates, 2-mercaptobenzothiazole, para-chloro-meta-xylenols, silver-based compounds, chlorhexidine, polyhexamethylene biguanide, n-hyalamine, triclosan, phospholipids, Iodine, bromine, hydrogen peroxide, chlorine dioxide, ozone, vegetable oils, plant extracts, chlorine, and the like. , Sodium hypochlorite, fenesol, inulin, prebiotics, benzalkonium chloride, and combinations thereof. The article may be in the form of a film, and in one potential application, it may be disposed on the absorbent article. |