http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170015878-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-16 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-86 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 |
filingDate | 2015-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81ade8536c2e3a373f351b97825a1088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7733cb75c166a279cacdfcf72d016d08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d92609a1a254d5bc40fa2957bd982714 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a259836142fbbf0fea6f8f5fe2cef677 |
publicationDate | 2017-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20170015878-A |
titleOfInvention | Terminally modified polyethylene terephthalate resin, method for producing same and molded article |
abstract | Modified polyethylene terephthalate resin having an intrinsic viscosity of 0.5 to 1.8 dl / g, a melting point of 245 to 270 ° C, a melt viscosity at 300 ° C (Pa · s) satisfying the following formula (A) And 25 to 80 mol / ton of the compound represented by the general formula (B) is bonded to the terminal thereof. 占? 4 占 e (0.000085 占 Mw ) (Note that the weight average molecular weight Mw used here is determined by gel permeation chromatography using hexafluoroisopropanol (added with 0.005N sodium trifluoroacetate) as a mobile phase, relative weight average molecular weight relative to the molecular weight of methyl polymethyl methacrylate Molecular weight) (In the formula (B), R 1 represents at least one member selected from the group consisting of an alkyl group having 1 to 30 carbon atoms, a cycloalkyl group having 6 to 20 carbon atoms, an aryl group having 6 to 10 carbon atoms, and an aralkyl group having 7 to 20 carbon atoms M is an integer of 1 to 3; n is an integer of 1 to 29; and X is H and / or CH (CH 2) 2 , and R 2 is a group selected from the group consisting of a hydroxyl group, a carboxyl group, an amino group, a silanol group, 3 , Y is H and / or CH 3 , and the total number of carbon atoms excluding the carbon atoms of R 1 and R 2 is 2 to 58) There is provided an end-modified polyethylene terephthalate resin having a low melt viscosity. |
priorityDate | 2014-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 179.