Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e5ad8562c578b061df7a2c3aee9d0e24 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-131 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-587 |
filingDate |
2015-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b1d3a1d700b69ac8bc375b1e6111532 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf12bde9eee9fa8c2eaf5c9d7f9d01db http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_831ee7c62a5a05d31a3e8053e3eb7850 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45e82c0f713b7c035f6dc5c9842dc0a7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_894d2d6b2f364e5b1bbd0aca4d1e1aaf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f129130c63878db4dbd1fa48873ec590 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c21441c4356292d7ccccd988bdbd5e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05b43dea555672e41754ddcf0a601a20 |
publicationDate |
2016-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20160113811-A |
titleOfInvention |
Preparation method of lithium titanium oxide particles coated with carbon and nitrogen, electrode active material and lithium secondary batteries |
abstract |
The present invention relates to a method for preparing lithium titanium oxide, which comprises mixing lithium titanium oxide and an aliphatic amine and refluxing at 80 to 120 캜 to coat an aliphatic amine on the surface of lithium titanium oxide; Centrifuging the mixture to obtain a solid fraction; Drying said solid matter; And carbonizing the dried solid material to prepare a lithium titanium oxide-carbon-nitrogen composite material containing a carbon coating layer derived from an aliphatic amine and a nitrogen doped layer on the surface of lithium titanium oxide (Li 4 Ti 5 O 12 ) And a composite material produced by the method. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107919461-A |
priorityDate |
2015-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |