A thermoplastic, refractory plastic molding material having improved mechanical properties and improved surface properties, especially for use in LDS, is described. (A) from 50 to 90 wt% of a partially aromatic, partially crystalline polyamide or a mixture of such polyamides, (A2) from 5 to 50 wt% of polyphenylene ether, or a mixture of such polyphenylene (A3) 0 to 40 wt% of a partially crystalline, aliphatic polyamide or a mixture of such polyamides, wherein the sum of (A1) - (A3) is 100 wt% of component (A); (B) 15 to 60 wt% glass fiber; (C) a mixture of an LDS additive or an LDS additive 0.1 - 10 wt% - the at least one LDS additive comprises an inorganic compound of wholly or partly copper and / or tin; (D) 0 to 40 wt% of particulate filler other than (C); (E) 0 to 5 wt% of further different additives, and the sum of (A) - (E) is 100 wt%. |