abstract |
The present invention relates to a binder resin comprising pores having a maximum diameter of 0.3 mm to 1.5 mm; And an airgel dispersed in the binder resin, wherein the volume thermal capacity measured by ASTM E1269 is 3,200 KJ / (m 3 K) or less, and a method of manufacturing the porous polymer resin layer. |