http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160046938-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33f8096f7c6f74ac787c777aaf01104a
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C19-03
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C16-00
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C4-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C1-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22F1-11
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C27-06
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22F1-11
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C27-06
filingDate 2014-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d84b7409d1d89ea44b5f4f07ab6d82e3
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_efbb9af722dee2e11431cb0edbb7e27c
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e664413e48e6ac38dc879ef0d36263a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_41bc5940475b87c6367bacc014367400
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd43496af9cf8005be70041f9a3ae5b8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1bea1787e2b081d0aa76661e52e5919a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aedcc166185ce1cce61cc4b8f3bfdc8e
publicationDate 2016-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-20160046938-A
titleOfInvention Cr-Al binary alloy having excellent corrosion resistance and the method for manufacturing thereof
abstract The present invention relates to a chromium-aluminum binary alloy having excellent corrosion resistance and a method of manufacturing the same, and it is an object of the present invention to provide a chromium-aluminum binary alloy containing aluminum (Al), chromium (Cr) remainder and unavoidable impurities in an amount of 1 to 40% Mixing and dissolving a raw material containing aluminum (Al), chromium (Cr) remainder and unavoidable impurities in an amount of 1 to 40% by weight based on the total weight of the chromium-aluminum binary alloy having excellent corrosion resistance, (Step 1); And a step (2) of solution-treating the alloy dissolved in the step (1). The present invention also relates to a method of producing a chromium-aluminum binary alloy excellent in corrosion resistance. The chromium-aluminum binary alloy according to the present invention has high applicability as a coating material of a material which is easy to manufacture, has ductility, and is required to have high temperature corrosion resistance and abrasion resistance. In addition, since it has excellent corrosion resistance not only in the normal operation of the nuclear power plant but also in the accident situation, the economical efficiency of the nuclear power generation and the accident safety can be greatly increased.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019098665-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11118260-B2
priorityDate 2014-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005154836-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H03211248-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID104727
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419491804
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5359268
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23976
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451324658
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419583196
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458391465
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3034927

Total number of triples: 35.