Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06F2203-04103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2250-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2457-208 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06F3-044 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06F3-041 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G06F3-041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G06F3-044 |
filingDate |
2015-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17c09c2628b0222d7efcde29ef0e3410 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_553df3ad0cabd1ae1284c5c1b65cc02c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b4b183bd25b2caa6ec277fbdae50518 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7d12915bcbc9329a4427789e9cda9da6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_835af0e12727ab75434b51715faa9bd3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aef76480c5f4e177d3159669d7a94892 |
publicationDate |
2016-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20160014551-A |
titleOfInvention |
Laminate, conductive laminate and touch panel |
abstract |
In the present invention, even when the adhesive layer attachment film is bonded to a surface of the base film opposite to the transparent conductive layer side and subjected to a heat treatment, the adhesive layer attachment film is peeled off, Is increased so as to appropriately prevent deterioration of the adhesiveness. A transparent conductive layer having at least one optically functional layer on one side of the base film and a low contact angle layer on the other side of the base film and patterned on the side of the optically functional layer opposite to the base film side, Wherein the adhesive layer-attaching film is attached to the surface of the low-contact layer and heated at 150 DEG C for 60 minutes, and thereafter the adhesive layer-mounting film is peeled off, And a wet tensile strength specified by JIS K6768 (1999) is 30 mN / m or more. |