http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160013772-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d21d8c00109933795105d295102ec426 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D7-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L79-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2014-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b30e612ca15e763c057fa5b04e5fe905 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed8eb801867a93f04997b566a5ce1361 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0a325ae04428039c3d70ddd65b51804c |
publicationDate | 2016-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20160013772-A |
titleOfInvention | Preparation method of polyimide film, and the polyimide film thereby |
abstract | The present invention relates to a process for producing a polyimide film by colorless and transparent polyimide by imidizing the polyamic acid solution at a relatively low temperature and then using the polyimide to form a polyimide film which is colorless and transparent as well as flexible and can be used for display purposes The present invention relates to a process for producing a polyimide film and a polyimide film produced by the process, which comprises the steps of: (a) preparing a solution of polyamic acid by adding dianhydride and diamine into a solvent, step;n(b) adding a chemical dehydrating agent and a catalyst to the prepared polyamic acid solution; (c) preparing a polyimide solution by imidizing the polyamic acid solution at 20 to 80 캜; (d) applying the prepared polyimide solution to a substrate; And (e) drying the applied polyimide solution to produce a polyimide film; . |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022004857-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2019286281-A1 |
priorityDate | 2014-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 182.