abstract |
The present invention relates to a composition comprising 10 to 20 parts by weight of a magnesia phosphate complex, 1 to 5 parts by weight of fly ash, 40 to 70 parts by weight of pulverized magnet, 5 to 10 parts by weight of potassium phosphate, 1 to 3 parts by weight of boric acid And 5 to 10 parts by weight of water. INDUSTRIAL APPLICABILITY The artificial stone composition and the manufacturing method according to the present invention can reduce the carbon dioxide emission by using the magnesia phosphate complex without using cement, and environmentally friendly because it does not emit volatile organic substances, increase the adhesion and durability, The cost of construction can be reduced, and the maintenance cost after construction can be reduced. |