http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160003601-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-18 |
filingDate | 2015-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa5709cf65976ebe34d2f30b796de1ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5936013f8e633fef85f5074b3f1729cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ccdb0cc1f186e3fe74ef792592184d7c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_45f25c4b77b503a4cab8947b306ef386 |
publicationDate | 2016-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20160003601-A |
titleOfInvention | Elastic diene terpolymer and preparation method thereof |
abstract | The present invention relates to a ternary elastomeric copolymer capable of simultaneously satisfying excellent mechanical properties and elasticity (flexibility) and a method for producing the same. The ternary elastomeric copolymer is a copolymer of 40 to 70% by weight of ethylene, 15 to 55% by weight of an alpha-olefin having 3 to 20 carbon atoms and 0.5 to 20% by weight of a diene obtained in the presence of a transition metal catalyst (i) a weight average molecular weight measured by GPC of 100,000 to 500,000, (ii) a pattern viscosity (ML) and a pattern relaxation area (MLR) measured by a pattern viscometer (1 + 4 + 2 a) . |