Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-122 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-621 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-624 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-386 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-13 |
filingDate |
2015-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d5cd1edd6be82de0696b6dfe60f77549 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a0b78c7bc505d029e8602da8870fdf30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b42e0fb54d7c33cca481644cad04d874 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2aa5b423706dc4d22366f001c24e3150 |
publicationDate |
2015-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20150124928-A |
titleOfInvention |
Anode active material slurry, preparation method thereof, and anode comprising the same |
abstract |
The present invention provides a method for producing a negative electrode active material, comprising the steps of: preparing a negative electrode active material solution containing a negative electrode active material, a solvent and a surfactant; And a step of adding a binder and a conductive material to the negative electrode active material solution, and a negative electrode active material slurry produced thereby. According to the method of manufacturing the negative electrode active material slurry according to an embodiment of the present invention, the negative electrode active material is dispersed first using the surfactant, and then the conductive material and the binder to be injected thereafter can be more evenly dispersed. In addition, due to such even dispersion, the adhesive strength of the electrode and the room temperature and low temperature output characteristics of the secondary battery can be improved. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180133749-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10693122-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114730864-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017171335-A1 |
priorityDate |
2014-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |