Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4a7711656877c108fcffc1b2b52cfc4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-40 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 |
filingDate |
2013-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_33a0e9694cfa2eb602631736ba5fd4c0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_343d4bcf62954dfab7c334c78bb35bf6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7bde936e7d042a639860d7cd3b4a800b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_67437708d4975f9cfd8949e559c7caba |
publicationDate |
2015-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20150080376-A |
titleOfInvention |
a method for preparing cathode active material, a cathode active material prepared thereby, and a lithium secondary battery including the same |
abstract |
The present invention relates to a cathode active material for a lithium secondary battery, a method for producing the same, and a lithium secondary battery comprising the same. The present invention relates to a method for preparing a composite metal oxide, comprising: providing a mixture of a precursor of a composite metal oxide and a lithium compound; subjecting the mixture to a primary heat treatment at 670 to 750 ° C for 2 to 5 hours; And a third heat treatment for cooling the second heat-treated mixture to 100 ° C. According to the present invention, a cathode active material having a small amount of LiOH on its surface can be produced, and a lithium secondary battery improved in capacity and lifetime characteristics can be realized by using the same. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111902365-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019198944-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220079728-A |
priorityDate |
2013-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |