Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ac092a42d435237ef56624ae229e9f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2aba27b15aa35b05768f4944055e8abe http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_99f3615dcb0af6d3a9721d2f0930a3ef |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-05 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-085 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-143 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-32 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B9-04 |
filingDate |
2013-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_160024e7ba73a1eb8ece646760032aa6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_012d35faf8526e64fab15cee9a28cff1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff3d1c967888172001443c7de119ba01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b96bf60210665a11eb3cba3aec6108db http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7968b61e26206391c38987a7ebfd187 |
publicationDate |
2015-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20150076998-A |
titleOfInvention |
High early strength concrete composition unnecessary for steam aging |
abstract |
A concrete composition for early strength development which does not require steam curing which can secure a strength of 10 MPa or more within 6 hours of curing without adding steam curing to the boiler without changing the physical properties of the cement by adding the curing accelerator at an optimal content ratio do. The concrete composition for early strength development which does not require steam curing according to the present invention is applied to crude steel cement and is a concrete composition for early strength development that does not require steam curing to exhibit a compressive strength of 10 MPa or more within 6 hours of curing without performing steam curing Wherein a hardening accelerator is added in an amount of 5 to 8 parts by weight based on 100 parts by weight of the crude steel cement. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114891163-A |
priorityDate |
2013-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |