abstract |
(A1) at least one semiaromatic, semicrystalline polyamide having a melting point of from 250 캜 to 330 캜, and (A2) at least one caprolactam-containing polyamide which is different from at least one semiaromatic, semicrystalline polyamide (A1) and which has a caprolactam content of at least 50% by weight; Containing (A) 27-84.99 wt% polyamide mixture, (B) 15-65 wt.% Of at least one filler and a reinforcing agent, (C) 0.01-3.0 wt% of at least one thermal stabilizer, and (D) 0-5.0% by weight of at least one additive, The total caprolactam content, i.e. the sum of the caprolactam contained in the polyamide (A1) and the polyamide (A2), is 22-30% by weight, based on the polyamide mixture, It is possible to add up to 100% by weight of the components (A) - (D), and that the metal salt and / or metal oxide of transition metals VB, VIB, VIIB or VIIIB of the periodic table are not added to the polyamide molding composition By weight based on the total weight of the composition. |