abstract |
To provide a hydrogenated block copolymer pellet which is free from blocking between pellets and which is excellent in transparency, flexibility, bleeding-out property and low combustion amount. 100 parts by mass of the pelletized molded article of the hydrogenated block copolymer A and 0.01 to 1.5 parts by mass of the kneaded powder of the polyethylene-based powder B, wherein the hydrogenated block copolymer A is a block copolymer comprising a vinyl aromatic monomer unit- , And the total amount of 1,2-bond and 3,4-bond before hydrogenation is 40 to 90%, and at least one polymer block (b) having a conjugated diene monomer unit as a main component, and the hydrogenated block copolymer The hardness of A is 30 to 67 °, the content of the polymer block a in the hydrogenated block copolymer A is 5 to 30 mass%, the number average molecular weight of the polyethylene-based powder B is 15,000 or less, 1 to 15 [micro] m and an angle of repose of 45 to 70 [deg.]. |