Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0094 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0091 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-056 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-056 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 |
filingDate |
2013-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9525dd9478cce82ab5b31edb2bcd13a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_70506f267d52c854ab75c7b50dfec2f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c92fe81186b4a5cfbbc3818de38a1e4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_815a788fc663ce15f241ae3b9303d66c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99fc94cb7d945fb6309758d144f9c51b |
publicationDate |
2014-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20140146934-A |
titleOfInvention |
Capsulated electrolyte having layer structure and method for preparation |
abstract |
The present invention relates to an encapsulated electrolyte having a layered structure and a method for producing the encapsulated electrolyte. More particularly, the present invention relates to an encapsulated electrolytic solution having a layered structure formed by capsules containing an electrolytic solution, Wherein the capsules have an average particle size of from 1 to 10 mu m and an average coating thickness of from 0.1 to 2 mu m and wherein the weight ratios of the capsules having an average particle size and an average coating thickness are in the range of To about 50% to about 95%, and a method for producing the same. According to the present invention, there is no need for a separate step of injecting the non-aqueous electrolyte, so that the manufacturing process of the secondary battery can be simplified, the impregnation of the electrolyte can be uniformly performed on all the surfaces of the cathodes, the anodes and the separators, Safety is improved. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107331894-A |
priorityDate |
2013-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |