Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2467-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2301-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3033 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-08 |
filingDate |
2014-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_76bee357ece93dcf28218711dc83d12b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4267031d6b9901e58354f62431abbcb6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_401ccc66b26605ed4dfb943190e9da98 |
publicationDate |
2014-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20140113472-A |
titleOfInvention |
Cellulose acylate film, polarizing plate and liquid crystal display device |
abstract |
assignment A cellulose acylate film having a small thickness is capable of exhibiting a desired retardation and is free from irregularity in condensation. Solution A cellulose acylate having a total acyl substitution degree of 2.60 to 2.95 and at least one polycondensation ester containing an aromatic dicarboxylic acid residue and an aliphatic diol residue are contained in an amount of 35 to 100 parts by mass relative to 100 parts by mass of the cellulose acylate , The proportion of residues containing an aromatic group relative to all the dicarboxylic acid residues in the polycondensation ester is 40 to 100 mol%, the film thickness is 20 to 80 mu m, and satisfies the following expressions (1) and (2) Cellulose acylate film. (Formula 1) 30? Re (550)? 100 nm (Formula 2) 90? Rth (550)? 170 nm |
priorityDate |
2013-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |