http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20140091806-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_379c1c9dec567dbf1ef1f425af59552e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-40 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-128 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-121 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-2623 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-36 |
filingDate | 2013-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_397abd6baa2d9157f0aedd2d2a79214d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_addaa3a71150b1944d6fca464405e7e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7bf2a093fb213552557cd927ff30bdb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_888d07e6dbb76d0249e7f199adb64087 |
publicationDate | 2014-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20140091806-A |
titleOfInvention | Modified sulfur binder and the method for preparing thereof |
abstract | More particularly, the present invention relates to a modified sulfur binder and a process for producing the same, and more particularly, to a modified sulfur binder and a process for producing the same, To 200 parts by weight of a heterocyclic amine modifier, an alkyl amine modifier, or a combination thereof, wherein the dicyclopentadiene modifier is selected from the group consisting of 1) dicyclopentadiene dicyclopentadiene (DCPD), or 2) a mixture in which at least one of cyclopentadiene (CPD), DCPD derivative and CPD derivative is added to the DCPD, or 3) dipentene, Wherein at least one of vinyl toluene, styrene monomer, dicyclopentene, and acyclic diene compound is added, wherein the heterocyclic amine modifier is at least one selected from the group consisting of: Pyridine, an isomer of pyridine, an isomer of an analog of pyridine, quinoline, isoquinoline, acridine, pyrrole, and N, And a heterocyclic amine containing S, and to a process for producing the same. The modified sulfuric acid binder according to the present invention is excellent in dispersibility, and therefore, when the modified sulfuric acid binder is supplied in the form of liquid, powder or emulsion using the same, higher solubility and improved dispersibility can be obtained during the hydraulic reaction. The mortar or concrete product characteristics can be made more uniform and good, and further, the modified sulfur binder in the form of powder or emulsion has a very convenient advantage in storage and use in actual field. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101658893-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102260685-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110183148-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102561622-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102032130-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102335008-B1 |
priorityDate | 2013-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 122.