abstract |
The present invention (A) 29 to 89% by weight of at least one polyarylene ether sulfone having an average number of phenol end groups per chain of 0 to 0.2, (B) 0.5 to 20% by weight of a thermotropic polymer, (C) 0.5 to 10% by weight of a polyarylene ether mainly having OH end groups, (D) from 10 to 70% by weight of at least one fibrous or particulate filler, (E) 0 to 40% by weight of additives or processing aids, Wherein the sum of the weight ratios is 100% by weight based on the thermoplastic molding composition. |