http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20140071414-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2310-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2230-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-6856 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4238 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-916 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-685 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 |
filingDate | 2012-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_735f3d37710420aee21ca47b15a198fa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23e76fcdc69a819709e1bf0f15645957 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0c45e0f80fe20f3d07338d449484127 |
publicationDate | 2014-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20140071414-A |
titleOfInvention | Method for producing aliphatic polyester having increased molecular weight |
abstract | An object of the present invention is to provide a method for efficiently producing a high molecular weight aliphatic polyester with high quality. In order to achieve the above object, the present invention provides a method for producing a polyurethane foam, which comprises (i) a mixing tank having a pressurized portion of a diisocyanate, wherein a number average molecular weight is 5000 or more and a terminal group is a hydroxyl group, Wherein the aliphatic polyester prepolymer is melted at a temperature not lower than the melting point and is in a liquid phase, (ii) a step of introducing an ester prepolymer into the aliphatic polyester prepolymer at a temperature higher than the melting point of the aliphatic polyester prepolymer, A step of press-fitting a diisocyanate corresponding to 1/10 to 2 equivalents from the press-fitting portion, and (iii) a step of reacting the aliphatic polyester prepolymer with a diisocyanate to produce a high molecular weight aliphatic polyester to provide. |
priorityDate | 2011-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |