http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20140040625-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b6b5f6c667accdd7bc86416835388aa |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2457-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2038-0076 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B38-0036 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B38-164 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-308 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-08 |
filingDate | 2013-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dea11e74b28e5e3284f4ac9ee449eb80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cd401706d77368ea3e494a1605282fa0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3223f8598e7eb1a8e2e004a798888822 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7dd386e52cf512fde8cdc36a529d5367 |
publicationDate | 2014-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20140040625-A |
titleOfInvention | Manufacturing Method of Laminate and Laminate |
abstract | The present invention can prevent the generation of bubbles when bonding to an adherend having a step on the surface, and after the ultraviolet irradiation, the endurance test was performed under high temperature and high humidity environmental conditions such as 85 ℃, 85% RH, using an oven. The present invention provides a method for producing a laminate and a laminate in which a laminated film using a photocurable resin composition having no turbidity even after being taken out of the oven and bonded to an adherend having a step on the surface thereof. (A) 5 to 10 parts by weight of at least one of (B) a hydroxyl group-containing (meth) acrylate monomer and (C) a photopolymerization initiator 0.5 (D) a bifunctional crosslinking agent in an amount of 0.1 equivalent weight or less based on the crosslinking point of the polymer, and having a storage elastic modulus (G ') at 24 ° C and 1 Hz of 1 × 10 4 Pa And less than 9 x 10 < 4 > Pa. |
priorityDate | 2012-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links