Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_17c6c7da627b7bead7208250127b52c2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S977-773 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2982 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B25-322 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B25-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L24-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L31-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L24-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B25-32 |
filingDate |
2012-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_583fa0650c7f5f66e71b4d1fe03d6aa9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_188cc225b008367b0f8dc34b55ba78f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed89da6a9244a92c9df14fc33e408f6f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0c5a31d3b9fa891bda02cd37affe2c79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5746f18d6296e64b144ab54292dd2fd8 |
publicationDate |
2014-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20140020605-A |
titleOfInvention |
Wheat Rock Kite and Manufacturing Method Thereof |
abstract |
And a process for producing the same. The method for producing hydroxycitic acid comprises the steps of adding a calcium ion supplying substance to water and a cation supplying substance containing a cation (X) other than the calcium ion to form a cationic aqueous solution, and adding a phosphoric acid supplying substance to the cationic aqueous solution Followed by aging. In the cation aqueous solution, the cation (X) may be included in an amount of 10 to 50 mol% based on the total cation (Ca + X). The phosphoric acid feed material may be added such that the molar ratio of anion to cation (anion / cationic = P / (Ca + X)) is at least 0.6. By the above-mentioned method for producing a hydroxocitrite, a high-purity hydroxycarboxylic acid having excellent crystallinity can be formed in a large amount in a simple process. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210090845-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210128985-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102236992-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021107325-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102248415-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220055550-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210052399-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210067984-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022250492-A1 |
priorityDate |
2012-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |