http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20130116455-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a9c8be5926503f1c3cb4dbcce92afd13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_040f855e83b53e24679ca5237ebaa4ec |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-46 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-08 |
filingDate | 2012-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_308cabf87764b595e05de1c279b023f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_97e707c2a3afbd5f510228ab180a03d6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_28ff4084d3c94f0b403e094a7864b438 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_137b5a7554b5f120ee310c7b72fa9626 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50989fde700541be9a083d68667d153a |
publicationDate | 2013-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20130116455-A |
titleOfInvention | Active carbon-transition metal oxide for electrode active material and manufacturing method of the same |
abstract | PURPOSE: An activated carbon-transition metal oxide composite electrode active material and a manufacturing method thereof have a super capacitor electrode with high specific capacitance and energy density by using an activated carbon-transition metal oxide composite active material as an anode or a cathode. CONSTITUTION: Porous activated carbon powder having multiple porous is prepared. The porous activated carbon powder is oxidized by being precipitated in an acid solution. The acid solution with the oxidized porous activated carbon powder is added in a transition metal oxide precursor solution. A deposit is obtained by titrating an alkali compound in the transition metal oxide precursor solution with the porous activated carbon powder. A material that a transition metal hydroxide and the porous activated carbon are compounded is obtained by selectively separating the deposit. A nanocomposite is obtained by thermally processing the material that the transition metal hydroxide and the porous activated carbon are compounded under oxidizing atmosphere. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114620722-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114620722-B |
priorityDate | 2012-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |