http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20130095294-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e015bdbcd472938c1ac1b34ca2f94ddc
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0445
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-28
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-049
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-26
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-52
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-32
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-131
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1391
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-28
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-044
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1391
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-131
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-28
filingDate 2011-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ddf861f39c4a8a28a99e462c2680dce
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1521eace69031fa34abf22a08e6d4704
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2be788cb274bd491256c525902621fbb
publicationDate 2013-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-20130095294-A
titleOfInvention Cathode for alkaline storage battery, its manufacturing method, and alkaline storage battery
abstract An object of the present invention is to provide a positive electrode for an alkaline storage battery and a method for producing the same, which can suppress an increase in battery internal resistance by uniformly coating a conductive material on the surface of the positive electrode active material particles and forming a strong conductive network. A method for producing a positive electrode for an alkaline battery includes: A) active material particles containing nickel hydroxide as a main component, the surface of which is coated with a conductive material containing at least one cobalt compound selected from the group consisting of cobalt hydroxide, tricobalt tetraoxide, and cobalt oxyhydroxide. Fixing to the current collector; And B) reducing the oxidation number of cobalt atoms in the cobalt compound to a state less than +2 by flowing a reduction current in an electrolyte solution to the current collector to which the active material particles are fixed after the step A.
priorityDate 2010-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID447822740
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID452951857
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID410553718
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID104730
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID13652349
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID164180967
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458391437
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6432046
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID61540
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451581551
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10129900
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID415729955
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID447676431
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID61534

Total number of triples: 42.