http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20130089596-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1837840b0d7f1d216335a0331a4bd15a |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-3281 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 |
filingDate | 2013-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_742073c78454878692defdc9c386f432 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_416b7efded9b60f12bf80ac046ea665b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_774e4ad3daa71f20604e5fd3818ad792 |
publicationDate | 2013-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20130089596-A |
titleOfInvention | Epoxy group-containing silsesquioxane modified epoxy resins, curable resin compositions, cured products, and coating agents |
abstract | (assignment) The present invention provides an epoxy group-containing silsesuccioxane-modified epoxy resin that is excellent in heat resistance and inorganic material adhesion and can form a cured product that does not lose adhesion to inorganic materials even under high temperature and high humidity. (Solution) It is obtained by dealcohol condensation reaction of a hydroxyl-containing epoxy resin (A) with an epoxy group and a silsesquioxane compound (B) containing an alkoxy group. The alkoxy group equivalent is 150-3000 g / eq, and the epoxy equivalent is 150-500 g / eq. And [molar number of epoxy group derived from component (A)] / [mole number of epoxy group derived from component (B)] (molar ratio) is 0.1 or more and 3 or less, and the weight ratio of component (A) and component (B) is a component ( B) / component (A) = 0.2-8, The epoxy group containing silsesquioxane modified epoxy resin (1) is used. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101986298-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015099443-A1 |
priorityDate | 2012-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 187.