abstract |
The present invention includes a polyester resin or a polyurethane resin, has an acid value (unit: equivalent / 10 6 g) of 100 or more and 1000 or less, a glass transition temperature of 30 ° C or more and 80 ° C or less, and a number average molecular weight of 5.0 × 10. Thermoplastic resin (A1) which is 3 or more and 1.0 * 10 < 5> or less, polyester resin, or a polyurethane resin, Comprising: The thermoplastic resin whose glass transition temperature is 0 degrees C or less, and whose number average molecular weight is 5.0 * 10 < 3> or more 1.0 * 10 < 5> ( The cured coating film containing A2), an inorganic filler (B), and the epoxy resin (D) which has a dicyclopentadiene frame | skeleton, dried at 130 degreeC for 3 minutes, and then heat-processed at 140 degreeC for 4 hours, At least the said thermoplastic resin At least one part of (A1) and the said thermoplastic resin (A2) relates to the resin composition for adhesive agents which takes a phase separation structure. |