abstract |
Disclosed are a method for producing a polymer, and a molded article thereof, which polymerize a monomer having a piperidine skeleton represented by the formula (1) or a mixture containing 0.01 to 35 mol% of the polymer at a temperature of 210 ° C or lower. [Formula 1] (In Formula 1, R 1 is a hydrogen atom or a methyl group, X is an oxygen atom, an imino group, or a specific oxygen atom-containing hydrocarbon group, R 2 and R 3 are hydrogen atoms, C 1 to C 8 straight alkyl group, C 1 to C 8 of A branched alkyl group, a C6 to C8 alicyclic hydrocarbon or an aryl group may be represented, and a ring structure may be formed with R 2 and R 3. ) |