http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120058547-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5198a2a21392d6cbc0bb4898b3fb3d29 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C28-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F21V7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 |
filingDate | 2010-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ebd08053b981584786b8c687561a5002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9fd9bd8b70b57d1b0df0b17afcee78b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da1b6ecbd4286535e59944dc085e7d81 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_db3b0637faf28d699ea96a0bfb1b5195 |
publicationDate | 2012-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20120058547-A |
titleOfInvention | Painted metal and its manufacturing method |
abstract | At least two layers including a first coating layer containing 35% to 70% of a rutile titanium oxide at a solid volume concentration on part or all of the metal surface, and a second coating layer laminated on the surface layer side of the first coating layer. In the coating metal plate which has a coating layer of, WHEREIN: The center line average roughness Ra of the interface surface of a 1st coating film layer and a 2nd coating film layer was 0.8 micrometer or more. Provided are a coating metal material having a much higher total light reflectance than the conventional one and excellent in formability, and a method for producing the same. |