Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K71-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-0076 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-1292 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B39-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B38-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-0084 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K71-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B38-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K71-191 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-1284 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K71-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B38-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B39-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B38-08 |
filingDate |
2009-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4115282f17f5e1971536912b4f625d94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ca009e69c4acf0d69ea98daae5c66aef |
publicationDate |
2012-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-20120051042-A |
titleOfInvention |
Methods and materials for manufacturing the contained layer, and devices fabricated using the same |
abstract |
A method is provided for forming a containment second layer over a first layer, the method comprising: forming a first layer having a first surface energy; Treating the first layer with a priming layer; Exposing the priming layer to radiation in a pattern to produce exposed and unexposed regions; Developing the priming layer to effectively remove the priming layer from the exposed or unexposed regions to produce a first layer having a pattern of priming layers, where the pattern of priming layer has a second surface energy higher than the first surface energy. Having); And forming a second layer by liquid deposition on the pattern of priming layers on the first layer. There is also provided an organic electronic device produced by the method. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10312443-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10756309-B2 |
priorityDate |
2009-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |