http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120045163-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_51306b7f585aca85f710dfe061f0f11e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23V2002-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23F3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23L33-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23P10-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23P1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23F3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23L33-00 |
filingDate | 2010-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f6196cfce74b2730c2537ce10dc821f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93bb5e306f020d434f20bddfb1c8736a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_32c3446385da59affced70b4a48af82b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ff3fa30ad170c20e57641ca537521b7 |
publicationDate | 2012-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20120045163-A |
titleOfInvention | How to Make Reed Rings |
abstract | The present invention relates to a method for producing a reed ring, pre-treatment step of collecting, washing and cutting the reed leaves and roots, put the pre-treated reeds in a cauldron or cylindrical pot and steamed for 6-15 minutes at a temperature of 150-250 ℃ After the first steaming process, the first steamed reeds evaporate the water and put it into a cauldron or a cylindrical kettle, the second steaming process to steam for 10-20 minutes at a temperature of 80-150 ℃, the second steamed reeds Or put into a cylindrical pot and a squeezing process to add aroma slowly at a temperature of 70-90 ℃ 30 ° C., a grinding process of grinding the scented reed tea to 100-200 mesh, the crushed reed tea Provided is a method for producing a reed ring, including a refilling step of molding a component into a ring after mixing the subsidiary material with the resin. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111631241-A |
priorityDate | 2010-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 40.