http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120041223-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bb5143c5d291d49c700ac1631bdd20df
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2982
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1317
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2201-21
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-61
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2201-54
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-57
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-131
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D1-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C49-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B15-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B29-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B19-095
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00
filingDate 2010-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57bf71f1a5cd00777cdfcabe8d234b2e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fa8233c4f4e20d49682a65150824b748
publicationDate 2012-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-20120041223-A
titleOfInvention Silica Powder and Silica Container and Manufacturing Method Thereof
abstract This invention is a manufacturing method of a silica container which has rotationally symmetry and has a silica as a main component, and has a gas containing bubbles in at least an outer peripheral part and an inner layer made of transparent silica glass formed on the inner surface of the gas. At least, as a raw material powder for forming the inner layer, the particle size is 10 to 1000 μm, containing Ca, Sr, and Ba at a total concentration of 50 to 5000 wt. Ppm, and the hydrogen molecules when heated to 1000 ° C. under vacuum. A silica container having a discharge amount of 3 × 10 16 to 3 × 10 19 molecules / g is prepared, and a silica container which is a raw material powder for forming an inner layer is formed. Accordingly, a silica container and a method for producing the silica container having a high dimensional accuracy and a thick transparent silica glass layer having substantially no bubbles in the inner wall and having high durability even at a high temperature at low cost, and a method of manufacturing the silica container Silica powder for producing the same and a method for producing the same are provided.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023080306-A1
priorityDate 2009-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID783
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID425193155
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24798
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449824900
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758

Total number of triples: 33.