http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120041209-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_38b04dac5e5700071e574cb587f8e099 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-18 |
filingDate | 2010-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee8e63038e66edac6baed87fdf91c66f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_256d416121043b6431deb161e5bf7024 |
publicationDate | 2012-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20120041209-A |
titleOfInvention | Flame retardant paint containing a cuprous oxide coating particle | grains, its manufacturing method, and the cuprous oxide coating particle | grains |
abstract | It is an object of the present invention to provide a cuprous oxide coated particle having high adhesion between the layer of nitrous oxide and the center material, good dispersibility in the flameproof coating, and high storage stability of the flameproof coating. In the cuprous oxide coated particle | grains in which the surface of a core material is coat | covered with the layer of a cuprous oxide, the said cuprous oxide layer completely covers the surface of the said core material, and is comprised from the collection of the octahedral cuprous oxide particle | grains. It is characterized by. This cuprous oxide coated particle is suitably manufactured by carrying out electrodeposition of cuprous oxide by maintaining pH of the electrolyte solution aqueous solution in an electrodeposition process at 7-13. |
priorityDate | 2009-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |