abstract |
The present invention is a resin mixture for melt processing comprising a first resin and a second resin, wherein the second resin comprises a polymer resin into which an organic functional group containing at least one oxygen is introduced, and a melt viscosity with the first resin ( Melt viscosity is a resin mixture for melt processing with a difference in shear rate of 100 to 1000 s −1 and a processing temperature of the resin mixture at 0.1 to 3000 pa * s, a manufacturing method thereof, and a resin molded article having a specific layered structure. According to the resin mixture, not only can the mechanical properties and surface hardness of the molded article can be improved, but additional surface coating steps can be omitted to reduce the process time, increase productivity, and reduce production cost. |