http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120006668-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7b2ea92ee7f2874a4a3ee0245a334ac7 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-005 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-80 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2010-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d1469fd245227d049ae05ee2e6e7a76 |
publicationDate | 2012-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20120006668-A |
titleOfInvention | Paint using natural mineral and manufacturing method thereof |
abstract | The present invention has good thermal insulation and flame retardancy, minimizes the release of harmful components generated from concrete or chemical adhesives, prevents the growth of harmful bacteria and fungi on the surface of the structure, and emits far infrared rays and anions. The present invention relates to paints using natural minerals that emit urea that helps to clean the air in the room or improve the health of the human body, and a method of manufacturing the same. The composition is 70 to 80% by weight of water: 20 to 30% by weight of ocher. After mixing, the precipitate was filtered to prepare Jiji water, and the wet ball mill was prepared with any one of 28 to 46% by weight of clay or mud, which is natural mineral of Jijisu and 80-120mesh particles, 4 to 7% by weight of sericite, and elvan 5 Rotational speed 40-50 to add -6% by weight, clinoptilolite 7.5-8.5% by weight, germanium 1.5-2.5% by weight so that the natural mineral is 325-1500mesh It consists of mixing 80-20 weight% of natural-friendly paint raw materials which were made by rotating by rotation of 20-50 hours of rpm, and rotation time: 10-20 weight% of normal paint resin. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101522076-B1 |
priorityDate | 2010-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |