http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20120005619-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6f932d94618d9b875e401457b33e9761 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2037-268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2305-30 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133528 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00644 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00788 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 |
filingDate | 2010-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be4e63535f079e3af43ff44fa6ae5b54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e39d13f3f32337933bf103712645bf8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7de51f4e179d98b31990ffbeeecaf96f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36c20a805cfac766dc4f784b307da033 |
publicationDate | 2012-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-20120005619-A |
titleOfInvention | Method for manufacturing antireflection film, antireflection film, polarizing plate and display device comprising same |
abstract | The present invention relates to a method of manufacturing an antireflection film, an antireflection film, a polarizing plate including the same, and a display device. Method for producing an antireflective film according to the present invention comprises the steps of coating an antireflective layer forming coating composition comprising a low refractive beads having a surface charge on a transparent substrate to form an antireflective layer; Attaching a release film to an upper surface of the antireflective layer and pulling the low refractive beads to orient the surface of the antireflective layer by peeling charging; And curing the coating composition for forming an anti-reflection layer. As described above, the present invention uses a coating composition for forming an anti-reflection layer including low refractive beads so that the low refractive beads are oriented on the surface by exfoliation charging so that the low refractive coating portion and the conventional high refractive layer corresponding to the conventional low refractive layer are provided. Corresponding to the high refractive index coating can be formed at the same time to reduce the coating process to improve productivity as well as having a simple structure and can be produced an anti-reflection film having an excellent anti-reflection effect. Therefore, the anti-reflection film produced by the above method can be usefully used for the polarizing plate and the display device. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016168688-A |
priorityDate | 2010-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 75.